Hi Fuzzi Shu,

    I use epoxy quite a bit in my work. The question I have for you, what
    kind of epoxy are you using? If you are using Devcon 2 part 2 ton,
    there should be no reaction whatsoever with the Haggerty. There are
    very acidic anti tarnish dips out there, and what their reaction to
    epoxy I can't say. I suggest making a series of tests first. 

    For my husband's one and only good dinner jacket, I made resin inlay
    buttons (looked quite cool, I must say), with sterling silver, 2 ton
    Devcon, some tumeric mixed in and some with yellow mustard powder.
    The coat with the sterling went to the dry cleaners with no ill
    effects. They of course have tarnished now and I will have to clean
    them with a polishing cloth. 

-k
Karen Christians
Cleverwerx
Waltham, MA
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project