    Personally, I have tried both - agree - it's ones preference. An
    interesting thing happened a couple of weeks ago. Being a PMC/Rio
    Certified, I get lots of inquiries about classes, etc. This
    particular one was different in that the lady wanted to color hers
    with Liver of Sulfur. OK - I was game, she had a bunch. I had the
    method that CeCe Wire uses - hot water, dissolve small pea sized LOS,
    dip while counting, rinse in clear water, etc. We heated water, made
    new solutions again and again, changed rinse water most often. (The
    bucket nearly runneth over!) These items had been fired elsewhere,
    but this gal knew which was the PMC 3 and the Art Clay (which # I
    don't remember). The same method of coloring was used for both and
    WOW, the Art Clay took the color immediately. 

    We did get gorgeous golds, bronzes, burgundy, peacock blue, slate
    gray up to the nearly black. The Art Clay was a little too quick to
    get the lighter colors but did get the darker ones. The illustration
    in CeCe's book shows what wonderful colors can be obtained in
    sequence. She has a great group to put on the market. I haven't
    contacted her to see how the colors are holding up. 

Rose Marie Christison
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project