Melissa,

    I would like to know what level of patina you are trying to preserve
    on your pieces. Are you trying to keep them a dark grey or are you
    trying to preserve some of the wonderful blues, golden browns and
    magentas you get at various stages? If you check the archives, you
    will see that I asked your very same question a while back. I got a
    good response to my query about what other people use to set their
    patina colors without dulling them and I tried many of the
    suggestions, Renaissance Wax, Nikolas Lacquer, and other sprays,
    etc, but I too found none of them worked as a fixative without
    totally dulling the beautiful colors I spent time and effort trying
    to achieve. I do continue to spray my patinaed pieces and
    unfortunately, am resigned to live with the dulling because I have
    seen pieces that were not sprayed - customers wearing them etc, and
    they look far worse - the patina just darkens and becomes very dull
    grey/brown and unattractive. I was hoping someone would come up with
    a terrific answer too and I am sorry I don't have one for you. Here's
    hoping...... 

Grace
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project