>     Is there a way to buff the scratch(es) out? There is one that is
>     across the front (side to side, against grain), she said they are
>     not very deep though. 

    As Frank Zappa once said 

    "rub it with a vigorous circular motion hitherto unknown to the
    people of this area, but destined to take the place of the mudshark
    in your mythology......Here it goes, the circular motion, now rub
    it!" 

    Although instead of using yellow snow, grab some coarse grit sand
    paper and create a new scratch pattern. Youll be suprized how
    difficult *small* scratches across a linear sanding line can be to
    get out. Plus it creates a cool new look that can take the abuse
    without having to touch it up. Granted if she has a matching stove,
    dishwasher, breadbox, toaster, blender, microwave, freezer, and
    storage bins, this might be an adventure. 

P AT 
www.patpruitt.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project