From: Leif M Date: Tue Feb 05 19:59:09 2008 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== My experience is that the coins don't crack when they're rolled out provided they're properly annealed. They do however tend to retain a "ghost image" of whatever was stamped on the coin even when it's rolled down fairly thin, say 1mm. I've had success getting rid of that "ghost image" with some minor filing or sanding. It may be possible to even just polish or lap it away with an agressive compound but I've never tried that. It's been a little while since I've rolled out a coin like that but as I remember it the silver was pretty good, no voids or anything as you can sometimes get when you're pouring your own plates in an ingot mold. At the time of wirting silver is at $16.73 per oz.so either way, it's a relatively inexpensive experiment and the worst case scenario is you have some silver to use in your next casting or any other number of projects. Hope this helps. Leif ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project