    I understand a bit of your dilemma. My mother who passes away last
    year had a favorite string of "pearls" - again glass beads about 3/4
    inches in diameter and a bit knobby. She loved them, but had macular
    degeneration a refused to throw them out, even though half the
    finish was gone. I considered trying the nail polish route, but had
    feelings similar to yours. I thought I solved the problem when I
    finally found another huge ugly strand at a second hand shop, but
    every so often I would see her in the old strand. Well, it made her
    happy so, since I was the one it bothered, I just let it go. 

    As an aside, much of the pearlized paint you see on cars actually
    uses ground fish scales for there finish. I spoke with a person who
    also said it was a common practice to use fish scales in a paint like
    matrix for fake pearls and mabe blisters. I think you should give the
    paint a shot. 

Marlin in snowy Denver - getting tired of this weather.
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project