========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Karen - Like everything else, using a tumbler takes a bit of education. This article from orchid archives http://www.ganoksin.com/orchid/archive/200601/msg00913.htm should help. My bias is to use products made for the process - a burnishing liquid would work much better than regular soap. Just steel isn't enough to get a decent finish on jewelry. This is a whole process just like hand finishing. First you have to smooth the jewelry - in a tumbler, you use a mild abrasive in some kind of media. Then the steel to burnish. And it can all be further refined in a dry media to achieve a smooth high polish. To clean up your mess, drain the dirty water, and run everything with a can of regular coke that no longer fizzes. Run for 15 to 20 minutes, then wash everything well with warm soapy water, rinse with clear water. Also, IMHO, 2 hours is way too long to run work in steel. I usually run for 30 or 40 minutes. Anything longer starts to degrade the surface. Judy Hoch ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project