    I would like to add my tcw to this thread. Although Sinkankas' book
    is a great resource for faceting and cabbing I have found a huge
    amount of info explained just ever so slightly differently in
    Christopher E Hyde and Richard A Matthews' The Complete Book of Rock
    Tumbling. This book has been invaluable to me as I have taught
    myself to cut, grind, create performs for tumbled finish and hand
    finishing, created pounds of hand broken tumble loads and so on. They
    do a wonderful job of thoroughly explaining processes, gives all
    kinds of technical and machine info, almost as good as Krey T's
    website! This book even takes you into the finish work of what kinds
    of settings and uses for your finished rock and the basic steps to
    creating them. For newbie's in lapidary work or for someone just
    adding that as a part of the whole jewelry making process this book
    would serve you well. I found mine for cheap on eBay but even new it
    would be worth the investment. Cori in Wisconsin where the rocks are
    still frozen to the ground!
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project