>     I don't think I have read in this bit of info about
>     soldering....the solder has to be as clean as the bezel and the
>     base. Solder oxidizes while it isn't being used. I pull the wire
>     solder through a 3M Scotchbrite pad before each use....I don't cut
>     snippets and store them, they also will oxidize. The same with
>     sheet solder, it should be cleaned before each use. Storing those
>     extra snippets will not be clean enough to flow. 

    That is a VERY good point. This also occurred to me yesterday as I've
    griped about solder and been on a quest for a particular kind of
    solder which I really enjoyed using. I remembered yesterday that when
    the said solder arrived with me, it was somewhat grimey as it was in
    the same bag as polishing compound among other things, so I washed
    the panels of solder and then pickled them too. Maybe that's why it
    worked better than anything else I've ever used! I spent about an
    hour the other day rolling solder strip thinner (as it was too thick
    to cut small pieces), cleaning it, pickling it and cutting it into
    tiny pieces then I stored it in jars. Now I've read your post, I'm
    thinking that that was probably a complete waste of time. Oh well. 

    I submit this post at the risk of looking and feeling a complete
    fool! 

Helen
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project