From: Helen Hill Date: Sun Jan 06 04:17:09 2008 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Beth, > If you are going to use PH down (sodium bisulfate), for your > pickle, keep in mind that this is a swimming pool chemical. It > regulates the PH in the water for pools and spas. So... the bottom > line is you need to dilute it, not neutralize it; no other > chemicals needed except more H2O. What you said is not really accurate. Yes it's a pool chemical and pool chemistry is quite complex with a number of reactions taking place, but simplified, chlorine based chemicals are generally basic or alkaline and as such need to be neutralised to regulate the pH of the pool, hence adding pHDown. pHDown is an acidic chemical which lowers the pH of the pool to neutral and therefore safe to swim in. Therefore using the pHDown as a pickle is effective because it's an acid so it should be neutralised with sodium bicarbonate or similar before being flushed into the water system. Most people have such a chemical in a cupboard somewhere in their house, either as baking soda or washing soda and if not it's on the shelves in the supermarkets. Helen UK ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project