Hi Janet,

    If we cast it, it was 3.5%. You may or may not remember that we
    tried to discontinue the platinum silver at one time. This was due,
    in part, to its tendency to be brittle for some applications. We
    were compelled to reverse our decision when many of our designers
    expressed their unhappiness with our decision, wanting instead to
    just deal with the limitations. That being said, I would never sell
    anything that I was unwilling to stand behind. If you want to return
    that bangle for metal credit you may. 

    On the news front, we have found a more consistent source for the
    3.5% grain a few months back and now offer the 1% as well. Also, we
    have invented a method for making waxes with the same resolution as
    the Hi Def material. The results are unbelievable! I can't wait to
    show it to you. I should be visiting the SF office later this month
    or early Feb. If you want you can reach me on my cell as I am out of
    the office today. I'll send that in a separate e-mail. Hope all is
    well. 

Jason
CH
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project