========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== This is not my favorite job for sure, but it comes up every once in a while. I find that when I see this type of setting job coming up it helps my focus to review a DVD I purchased some time back, "Bezel and Flush Setting" by Blaine Lewis. I did this type of setting work before I ran across Mr. Lewis' video, but I find adapting his techniques to my own style works quite well. If some one has little experience at this setting style his DVD would be a good starting point, I think. At least we're talking about flush setting in Platinum and not flush setting emerald or fire opal in 18K white gold: a REAL favorite of mine (note gray hairs)! ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project