========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Helen, I rarely polish anything at my bench. I hate getting my bench all dirty with compound. To get in crevices, I use Supra MK brushes from Gesswein, with their plastic spindle, which goes on the polishing machine. I use the 3/4 inch size in soft for silver, medium for gold. I keep a few of the 1 inch size for when I need to get into a really deep crevice. But I buy the 3/4 inch size by the gross, because I use them all of the time. I use them with tripoli, white diamond, and rouge. You do need to reapply the compound frequently. If you are nervous about the polisher, try using small buffs at first, maybe 3 inch diameter. They don't spin as fast as the larger ones. I love the PR88 hand protector cream, available from Stuller. It really keeps polishing compound from getting ground into your hands and nails, and washes off with water. Hope this helps! Lauren ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project