From: daniel spirer Date: Wed Jan 02 04:35:18 2008 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Teresa, Never had a problem with polish or finish (although getting the blue coloring that happens with soldering out of some of my detail was problematic). Just the soldering issue, sizing too as there is no solder I found that wouldn't show a seam. I don't do my own casting, but none of my casters seemed to be able to consistently produce pieces that I was entirely happy with. Maybe I'm just too fussy about some things. Plus ultimately it's just basically a cheap platinum substitute, so if it's the least bit problematic for me, why should I cheapen my work in general by offering it instead of platinum? But then my market supports those thoughts...I know it's not for everyone. Daniel R. Spirer, G.G. Daniel R. Spirer Jewelers, LLC 1780 Massachusetts Ave. Cambridge, MA 02140 www.spirerjewelers.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project