>     It's not the straight shape of the prong that's the problem. It's
>     the way the seat is cut. The OP described just a tiny drill hole.
>     That means a round hole, at least to me. So the hole, though it
>     traps the point, and would also prevent a stone from falling out in
>     the manner you describe in the rest of your post, does not equate
>     to a proper setting... 

    I agree with most of your response, however my point (no pun
    intended) was to challenge the assertion that settings other than
    V-prongs are incorrect. And no, I don't take whatever I
    read/watch/hear from "industry leaders" as gospel. Not that you're
    entirely implying that, but I'm going to say it anyway. There is
    certainly no better teacher than experience, but I'd like to avoid
    as many headaches as possible by learning from others. Ironically, I
    end up paying $$$ and time no matter how I continue to learn. Have
    they invented that "learning by osmosis" machine yet? :-)
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project