Re: [Orchid] Mokume gane thickness for domes  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: John Donivan
Date: Thu Dec 13 05:08:34 2007
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     I'd like to hammer the mokume gane sheet into a dome using a
>     dapping block and a punch. Is the 24 gauge too thin for this? 

    Jeunesse, I saw your first post, and thought others would pick up on
    it... As usual, there's not really an easy answer to your question.
    First off is what quality and weight you want to have. Second is what
    do you mean by a dome? If your dome is 1/2" wide then 24 ga. is
    perfect. If it's 4" wide it's so much too thin that it won't survive
    the process. All I can really say, partly because I really don't even
    use gauges anymore, is that I used to use 22 ga for most everything
    thinner, and 18 ga for most everything thicker. Again, if you're
    doming a 1/2" dome then 18 ga is too thick to even dome effectively,
    but for a 3" concha it's perfect. Thinner is going to be prone to
    denting later on, for one thing... Hope it helps, there's no "right"
    gauge for it, it's what you're looking for in the end.. 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project