========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Regarding solvent and evaporation issues: I use high grade Kimax- rubber coated and nalgene/vinyl gasketed glass bottles for solvents. They are superior to any metal cans and can be reused over and over with a soap and warm water wash.they are also unbreakable! If any one wants the supplier email me off list and I'll send the link. The cheapest available (that I know of) for a 1000ml bottle is 8 bucks for one piece. Additionally, Nalgene bottles,cans,pails and drums are leak and evaporation proof and come in a wide range of sizes, mouth styles and cap styles from metal and phenol with a pulp or vinyl insert to those with enameled coatings and chemical proof(wet and dry) inserts. Berlin packaging is the cheapest wholesale source, but has a division called Freund, that sells retail ( small quantities) and single items, as well as offers clearance and surplus sales on assorted storage containers. They will also beat any price with which you supply them from competitors or printed ads. I have used nalgene and kimax for years to store acids, solvents and other volatile, flammable, inflammable and hazardous materials and chemicals without leak, or evaporation, or breakage and recommend them both highly. R.E.Rourke ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project