>     ...The sprues shown are HUGE. The sprue for the pendant (the second
>     casting shown), must be at least 1/2" wide! I guess that explains
>     how it is done. 

    1/2" sprue! Having never seen the video (I didn't buy the kit, I just
    use the clay in my regular sand casting flask), that sounds way
    oversize to me. It may simply be a trick of perspective. I do use a
    much larger gate than you would use for lost wax, but it's more on
    the order of 3/16" to 1/4" (small drink straw size), but a 1/2 inch
    is something I might use to feed a multi-item casting in a very
    large flask. 

    On smaller castings, I've regularly used a golf tee to poke a gate
    through and gotten fine castings from that. Again, I've been doing
    this with bronze, old-school sterling, and occasionally brass. 

    On a gravity pour, your _button_ needs to be at least as 2/3 the
    mass of the casting itself, some people will say equal. 

Ron Charlotte -- Gainesville, FL
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project