From: Renaissancewiz Date: Thu Dec 06 04:58:30 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== It's possible that it's not the metal at all. You might want to try changing your hand soap and any creams or lotions that you're using. The list of chemicals in these products is downright scary, and allergies are very common. Of course the residue collects under your rings if you wear them constantly. Once you develop an irritation it seems to escalate at a pretty fast pace. That would be a nice solution to your problem. Best of luck to you. I'm very interested in finding out how this comes out. Be sure to keep us informed as you solve the problem. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project