[Orchid] Mokume gane still it will not bond  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: James Kallas
Date: Wed Dec 05 04:25:36 2007
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    A question for you mokume artists out there? I have a billet that
    has fused except for the middle section it is 18 Kt green 14 kt
    palladium white and 14 kt rose. the section that has not fused is 18
    kt green and 14 kt white and is dead center of the billet all the
    other layers have. I have fired this 3 times after thoroughly sanding
    and cleaning the surface, twice  AT  1225 deg F for 8 hr and once  AT  1525
    Deg F for 3 hr and still it will not bond, is there any thing that I
    can do to promote these pieces to fuse and will it hurt the metal to
    keep firing it? The rest of the layers seem to have fused solid and a
    prior billet the same dimensions of 22 Kt and shakudo gave me no
    trouble. Any advise would be greatly appreciated 

Thank you in advance James Kallas
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project