hi all...

    well, i just got married in september. my studio mate and friend,
    geoff giles, made my engagement ring which i have worn since
    february 2007. it is 18k palladium white gold from hoover and
    strong. 

    i made the wedding band. it is 18k palladium white gold from hoover
    and strong. 

    one band is 3mm, the other is 4mm. each one has 1.8-3mm diamonds all
    the way around. they are not too small, and i take extreme care to
    dry my hands after washing. i also do not work in my rings anymore
    in case some pickle or other irritants get trapped underneath. 

    i have developed some sort of allergy, where i have 2 distint bands
    of allergic reaction around my finger, which are red and sometimes
    blistery. i tried wearing the rings this morning as i was out and
    about at appointments, and my finger swelled and itched and hurt an
    hour after putting the rings back on after three days of not wearing
    them. i had to take them off. 

    what is the problem here? i thought i was safe since hoover's
    palladium white gold has no nickel! i am upset and confused. do i
    need to ---god forbid--- make new rings out of yellow gold??? 

    i also have to admit that i do not really wear jewelry, and this is
    the 1st time i have worn gold for any extended period of time. 

    any thoughts on this matter for me? 
    thanks so much! 

joanna gollberg
www.joannagollberg.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project