>     Cutting will not cause a diamond to cleave, but I have seen a
>     customers ring with a diamond that was hit just right, it was
>     still set, but the top had come off at an angle slanting downward
>     across the diameter. 

    The situation you are describing could happen. But if stone would be
    examined before setting the flaw is easily seen and I would reject
    such a stone. Any gemstone must be examined before setting. Also, the
    damage causing diamond to behave that way was introduced during
    cutting. Sometime they fell apart on the lap, sometimes setter is
    left holding the bag. That is why examination is critical. 

>     Great care in setting is not enough when the pressure needed to
>     move the metal is greater than the pressure needed to break that
>     particular diamond. 

    You hit the nail on the head. The key to safe setting is to never
    exceed the safety threshold. We are jewelers, we are not plumbers.
    The work is accomplished through the application of the intellect, 
not
    muscle. 

Leonid Surpin.
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project