From: vdl van der lijn Date: Mon Dec 03 07:35:59 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hello Marty, here a tip for using rolling mills. Have o look on the website of "DURSTON" on this address http://www.durston.co.uk/en/online-guide-p1-en.htm You will find a lot of useful tips, for the rest lets work your own fantasy to develop more. With a little practice, i am sure you will make better than you find in books, and much more personal. Succes hope i was from any help. Guy Rebecq Belgium Sorry for my English, i speak only Dutch and French. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project