========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Dear Jonathan, Any good zero or low-shrinkage rubber mold material will do what it promises to do -- produce a mold with zero or little shrinkage. But that's not what you are really interested in. What you really want is a zero or low-shrinkage CASTING. And that's not produced automatically by the simple choice of a mold material. Casting shrinkage (as opposed to mold shrinkage) is the result of 100's of factors introduced by the mold maker and the caster. Most of them are not even aware of the factors and just chalk it all up to "variability". Others know the factors involved but feel they cannot cope with them and still run a commercial operation. The only answer I know of is to find a good caster, figure out his shrinkage rates and size your waxes to give the results you want using his services. At least that way you'll have eliminated many of the variables caused by using different casters and their different procedures. Michael Knight Castaldo Products Mfg. Corp. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project