>     Is there a simple test to be sure the cyanide is completely
>     neturalized? Perhaps a drop of something added to a small am ount
>     in a test tube, that will change color? 

    According to my (rather old) Brepohl, in the context of disposing
    cyanide solutions from electro-plating jobs, he recommends the
    following proceduRe: 

    1. Put the cyanide solution into a plastic bowl 

    2. Add a 10..20% ferrous sulfate (FeSO4) solution until color
    changes to rost colored, later chartreuse (greenish-yellow). This is
    potassium ferrocyanide / yellow prussiate of potash - K4Fe(CN)6 

    3. Now add a 10% ferric chlorid (FeCl3) until the solution gets
    blue. This is Prussian Blue / Berliner Blau / Turnbull Blue /
    Eisen-hexacyanoferrat(II) - Fe7N18C18 

    According to the book, this is no longer toxic. And you have definite
    colors to know when you are there.
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project