========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > So I still am of the opinion that, even though it's not very > clever to heat diamonds to 900C, it is doubtful they would > actually disappear completely. Damaged, yes. Gone? No. This is a very interesting mystery. First of all, didn't you say that the diamond was in fact NOT damaged at all by two hours at 900C? The pictures of damage at 2800C are really interesting-- thanks for sacrificing the diamond! So, in re the original loss of the stones in the bar in the PMC-- we seem to have no choice but to conclude that they were in fact not diamonds, but clever simulants. People have been fooled before, and simulants have been around a long time (I think I recall that they were from a vintage piece). No one wants to believe that their diamonds are not real, but it seems to be the only explanation that encompasses all the info we have. Wait, now-- what metal was the bar they were set in? If it was not gold or plat, that would support the idea that they were not real diamonds. I love a good mystery! Noel ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project