========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > She has definately got plenty for a gold diamond ring, if that is > what she was into. She just always wears silver and that is what > she likes. Ali, much of the response to this falls in the category of conventional wisdom, and I agree with all of it. Especially if stones are involved, a silver ring is unlikely to survive the years anywhere near as well as gold or platinum. We do a LOT of bridal work, though, and I just don't argue with customers about what they want - if you explain to her the physical properties and pros and cons - informed decision and all that, and she still wants silver then so be it as far as I'm concerned. The objective facts about metal properties are all well and good, but it's her ring, more importantly it's her engagement ring, and that's that. If it were me I would take pains to make something that's built to last with the metal in mind - something delicate and pierced in silver will last two years, max, your basic 4 prong solitaire in silver will last 6 months till the tips are gone, stuff like that, but that's all... http://www.donivanandmaggiora.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project