========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Jennifer, S88 is the alloy manufactured by United Precious Metals for sterling silver. It is a low oxidation alloy that is all of the things that I believe a silver alloy should be. I solder this sterling using boric acid as a flux and get NO, Repeat NO fire scale. I cast and roll this alloy as well as forge it with hammers. It has a very white color ( I have had people in the jewelry business mistake the finished product for platinum because of the color) work hardens faster that regular sterling alloy (which I like) and will oxidize at a very slow rate compared to standard sterling. Casting properties are the best, I get beautiful castings that are virtually porosity free and come out of the flask white, not black or brown. What else can I say. It does not, at this time come in any other form than casting grain or pure alloy. I am trying to introduce this product to Stullers Settings and get them to add it to their line of milled (meaning wire and sheet) stock. I have posted about this alloy repeatedly and I think a lot of you are missing out on something great by not giving it a try.... United Precious Metals 1-80-999-fine . (usual disclaimer goes here) Frank Goss ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project