========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== When soldering or casting diamonds in place, the high temperatures are only held for short periods of time in a reduction atmosphere. When firing diamonds in PMC Standard, the temperature is held at 1650 for 2 hours in an oxygen rich environment. Diamonds do not survive this--they burn up in the kiln. When using the 3rd generation of metal clays (the low fire clays) and firing at a 10 minute firing schedule, reports indicate that diamonds will survive--whether the people reporting this have examined the diamonds closely for damage is unclear. Mary Ellin D'Agostino, PhD www.medacreations.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project