    I hate to beat the horse more but from all the questions about the
    draw bench and where to get winches and stuff I have to chime in
    again repeating some of my rolling mill post. 

    My first thought is if we look back in history the draw benches used
    at say the Faberge' shop were state of the art at the time.  I say,
    in my small mind that if they were still open they would not pull
    their own wire they 

    would buy it.  If they did pull their own wire they would have a
    $100,000.00 machine that draws the wire and anneals it all at the
    same time.  Why don't we all use hand drills instead of flex shafts
    they are just as good.  It seems like there is this little story
    going on in our heads that it is wrong to buy wire or stock, it is
    not a pure design if we don't make it ourselves. Faberge' did not
    have a metal house to buy from they HAD to make it.  If The House of
    Hoover was 2 blocks from Faberge' I guarantee that they would have
    used The House of Hoover later to become Hoover and Strong when
    Hoover left russia in 1917 after the March revolution and the
    abdication of the Tsar (sorry for the little humor and made up
    history). 

Keep busy everyone
Bill Wismar
www.metalbendersgallery.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project