From: Jeff Demand Date: Sun Oct 21 00:53:05 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Helen, A draw bench is only a luxury until you have one. Mine is a boat trailer winch and a bit of lumber, about 3 feet long. It lives hanging from the rafters and when needed is clamped in the vice. No expensive draw tongs, just a hardware store common slip joint pair of pliers with a steel ring over the handles. Cheap (mainly scrounge parts, decorative paint the greatest expense :-), and it doesn't take up space. Making big heavy wall tube is not only possible now but fun. Jeff ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project