>     It was probably asked already but how about welding with a wax
>     pen? You should be able to plunge that hot puppy into the join and
>     get a complete weld, no? 

    Several have mentioned sticky wax, whick obviously works fine in
    places. The problem is that it's thick and isn't right in some
    places. In the example I mentioned yesterday, which I actually cast,
    it was a triangle inside a circle, and all of the edges were around
    2.5mm wide. It needed to be put on a backing plate to be inlaid
    (obviously it could be carved fresh, but that's not the point)
    Another place I used it was putting wax letters or numbers down on a
    piece, like 25 year pins and stuff. You can go around all of those
    edges with a wax pen, yes, but it's a huge, messy job, and you can't
    get in the middle of it - you can only get the edges. If any
    investment gets underneath, which it will if there's any way for it
    (vacuum investing), it will blow the casting. That's where something
    more like a glue is needed, something thin and compatable with wax
    and burnout, and superglue does a good job of it, except again it
    doesn't have a lot of strength - glue it and leave it alone as much
    as possible. 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project