From: Daniel Wade Date: Thu Oct 11 02:57:07 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== You could also aquire graphite boards and place small drilled dimples in them. Put your torch to it with your cut pieces of metal in the dimples. For consistent size and large quantities of granulation beads I would recommend buying them pre-made. If you want to save a little money and do it yourself I would highly recommend getting pre cut lengths of wire. You would haft to measure the gauge and length of the cut so as to match what you make by hand. Lots of people offer the pre-made beads but we make cut to size wire and solder. I also notice people who put there torch to one side of wire when making headpins and the like. Sometimes it works but mostly the ball is off to one side and not even on the wire. Try heating from directly below the wire to get even heat distribution. Daniel Wade ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project