>     Now, the best solution to dealing with the near-ubiquitous ash is
>     to blow it out of the hot investment with an air gun, then return
>     the investment to the furnace for a minute or three to assure an
>     even re-distribution of heat before casting. I know what you're
>     thinking, but there has been no damage to the investment after
>     doing this many thousands of times. Sounds crazy, but it works. 

    Re Wayne's comment above. The problem with blowing out the mold - or
    any other closed cavity is that - the the offending material can't
    really get out very easily because the flow of air is going in. I use
    a vacuum cleaner, hose clamped in an upright position with a heavy
    piece of wide meshed screen over the end, on which I hold the mouth
    of the hot mold just prior to placing in the casting machine. This
    has proven immensely effective in getting out any loose investment
    particles or kiln insulation bits which have fallen in during
    burnout. 

    Do not try this without the "buffering" screen. Putting the hose end
    directly against the mold will actually suck out any thin investment
    formations and even the core section of a ring. Believe me. I know. 

Les Brown
L.F.Brown Goldwork
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project