From: Ag Smith Date: Sat Oct 06 04:24:36 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Thomas, > For silver dissolve it in nitric acid and precipitate out the > silver with copper. The result should be 99.9% pure silver (or > better if your silver was really clean prior dissolution as well as > the copper (use pure copper and it should be bright and shiny > clean too)). Would you expand a bit on how to precipitate the silver out of solution with copper? Dissolving in nitric acid is simple enough. ( and I understand the precautions necessary, toxic fumes, etc.) After the silver is in solution,in addition to the copper alloy already in the silver, how do you proceed to precipitate out the silver, and clean and reduce to pure metal? Thank you ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project