From: Peggy E. Pollak, Ph.D. Date: Mon Oct 01 06:39:35 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Please help. I've been casting for about seven years with someone else's oxy-acetylene set up with absolutely no problems and finally, this summer, got my own centrifugal casting set up. I opted for an oxy-propane torch since I was told it is cleaner. I've had nothing but problems since, most of which I will not bore you with, but now I use distilled water, with no change in the investment, waxes, or burn-out cycle. Recently I started to get these cement-like deposits all over my castings. It polishes out pretty easily with a 120 grit wheel but I lose alot of fine detail. Any ideas? Thanks. Peg ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project