========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     Aspect Ratio (AR) is the term. It is a handy little equation. If
>     you know that a weave will work with a given wire diameter 

    I thought I'd explain what this means to those casual readers who
    are just curious. If you have a 1mm wire, and make jump rings out of
    it to make either chains or chainmail with, then you have a decision
    to make. If the ID of your ring is 2mm, then you can maybe get 2
    rings to link to it, but your chain will be tight. If it's 3mm you
    can put two rings and you'll have a looser chain. Your basic
    chainmail pattern is called 4-in-1, which means that four rings link
    into one ring. So your ID for 1mm wire must be at least 4mm - if
    it's 6mm you'll get a looser mail. This all varies as to the size of
    the wire and the desired results, and that's what this all is about,
    is how to figure that out ahead of time. Many of the patterns have
    an optimum AR, because the links go together just a certain way, so
    it's even more important then. I'm not an expert at this, I just
    know about it.... 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project