From: Leland Baker Date: Sat Sep 08 07:06:35 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Thank you for the Paradise Wax Co. suggestion. I have looked at them and have already purchased what they have. Wilson ( or something like that out of Florida )..... they really didn't have anything. Great Western..... I can no longer reach. Lex Wax from K.C...... not really, but I am waiting for their new catalogue. Swest... was bought up by Stuller, so their items are no longer available. Unfortunately so many of the wax companies have gone under. So..... I guess I am looking for styles and individual waxes from across the board from individual jewelers. Wax patterns that individual jewelers already have from molds that they may have made of from previous jewelry. Potentially form items they have made for someone else when doing their jewelry. This is a good way for me to find patterns that are not mass produced and also a way for the individual jeweler to make money from resources just sitting around doing nothing. Leland ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project