>     I'd just like to throw my 2 cents in & mention that I clean my shop
>     with a vacuum brand named Rainbow Vac, It's not cheap, about
>     $1800.00. But it sucks the dust into a bowl of water & clean air
>     comes out the other end (Certified to be clean enough to be used in
>     an intensive care ward), All dust particles are deposited in the
>     water that You then empty. 

    The Rainbow Vac is not a HEPA vacuum. It will not do the job safely.
    The particles that you are concerned about are so small that they
    will not be thrown out of the air stream and will just flow with the
    air right on through past the water trap. What you need is a vacuum
    of the type used for asbestos removal they are very expensive and
    this is why wet mopping and wipe down is a more reasonable solution.
    Call the manufacturer and see if they will put in writing that their
    vacuum is certified for removal of asbestos or respirable crystalline
    silica, if not then do not trust that it is safe for this use.

James Binnion
jbin AT mokume-gane.com
James Binnion Metal Arts
http://www.mokume-gane.com
360-756-6550
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project