Hello dear Roberta,

    I am using an Optivisor from Carl Zessis (Germany),its magnification
    is 2X, I purchased it in Dec 1992,and since that time I am using
    it,and it is as good as new even today the lenses are in exellent
    condition even after so many years of continuos use. 

    I am 47 years old today and this above optivisor with 2X
    magnigfication was advised by an expert from Dental field, who said
    that this 2X magnification is best for the eyes for continuous use
    and I can say that he was right when he advised me 15 years ago, and
    i am using this optivisor since last 15 years with out straining my
    eyes.even today I use it for 8 hours daily for all my jewellery
    manufacturing work.. 

    The best thing about this above optivisor is its design of the frame
    which holds the lenses. It is very light weight and easily adjustable
    head band,and very durable,even after 15 years of use it is still
    like new. 

    I do not know if the above desigh is still available in Germany or
    not. If it is still available then i can highly recommend it to all
    who are working for 8 hours daily , any good quality optivisor with
    2X magnification and the lenses made form glass will equally serve
    the purpose. 

hope this will help
May all be Peaceful, Healthy and Happy.
Umesh
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project