From: Rick Copeland
Date: Tue Sep 04 06:56:54 2007
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     things you've tossed into a drawer or box and rework 

    When I decide I need to start over on a piece (usually soldering
    mistakes) I am usually so annoyed with myself that I take the flawed
    piece over to the bench shear and take out my bad spirit and cut it
    up. Or I put it on the anvil and hammer it into a pancake. 

    Maybe I should save the ones I hammer and attach a bale to it and
    call it "Rick's Angry Art" or "Rick's Therapy Art." ;-)

Rick Copeland
Silversmith and Lapidary Artisan
Rocky Mountain Wonders
Colorado Springs, Colorado
http://rockymountainwonders.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project