Hi Richard,

    Yes, it's glass. The original claim by the manufacturers of the
    material, sold to faceters by the ton, was that it contained ash
    from the eruption. It was available in at least 3 shades of green, I
    still have some here (I lived in WA at the time). Testing has shown
    that it does NOT contain any ash from the mountain, none. 

    I know who was making it and I know their sole agent at the time.
    His remark was "Well, we waved some ash over the melt, does that
    count?". It was trickery, designed to sell a bunch of green glass to
    faceters and to the public, and it worked. It's still happening,
    visit Sea-Tac airport sometime. The vendors will GUARANTEE it is
    made from ash from the eruption. 

    EVERYONE who has used ANY ash from this explosion as a glass melt
    additive has achieved the same result.....an opaque brownish glass.
    All attempts to make a glass or glaze from the ash. whether in a
    reducing, neutral or oxidizing environment yields opaque brown/black
    material. The whole thing is bogus. 

    The more recent material has a small amount of lead added to raise
    the RI, and it is very pretty. But, so is faceted Coca-Cola bottle
    bottoms. 

Wayne
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project