>     are the 3m bristle brushes superior can a natural bristle hand
>     brush with polishing compound be used for 

    Joel, if you want a good polished finish on any metal, cast or not,
    there are three steps - file, sand and polish, which has it's own
    steps involved. You're not likely to get a good polish by going from
    filing to a bristle brush - maybe with greystar or something, but
    that's awfully aggressive. The 3m brushes are nice - I don't use them
    a lot, but sometimes. What any jeweler will do is use the right tool
    for the job, so whatever works for you is best. I use what we call
    rubber wheels a lot, so I'm used to it - that's what we call the
    whole family of Cratex and Shofu and similar. Most 18kt is quite
    soft, so you can have problems with faceting, but you can also
    contour a lot on the polisher. In a nutshell, a bristle brush is
    probably not going to get you a good polish from filing, unless
    you're using #6 files. You'll have to work so hard it will probably
    degrade the piece. And the 3m wheels are probably a good choice for
    the sanding - not the only choice, but a good choice. 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project