    i have a hydroflux welder, and have used the spiritflame..It is not
    for beginners- unless your building's code restricts gas tanks..it is
    far easier to learn how-to with regular torches than the precision of
    a water torch, and the maintenance required is extensive relative to
    oxy/ fuel torches or air/fuel models. 

    as for used..i would remove the cover and inspect the inside hose
    connections for everything from corrosion ( there shouldn't be any
    whatsoever), and tightly fitted clamps and gaskets all intact ( no
    cracks, tears, splits, peeling, etc). the chamber covers should also
    be 100% clean, silicone seals clear and interior threads well seated
    without any signs of prying, cross-threading, or other damage. the o
    rings on the handpiece should be perfect, no breaks, stretching or
    otherwise damaged; they should be pristine. the torch handle should
    be opened and the interior brass filter checked, it drops out of the
    handle easily when opened, or give it a slight tap on the edge of a
    desk to dislodge it if necessary- if it is non-existent - don't but
    it, as the owner has not used it correctly..( most come with a spare
    filter cylinder).turn the machine on and look into the mixing chamber
    while its running and make sure it is nicely bubbling away..no
    bubbles and fluids show that they are at the proper level = a major
    problem..if the dryer material is gunked up or wet that is another
    bad omen.as would be the vinyl hose having moisture or algae
    visible.. those are the basics..write me off list if you want more
    info..i couldn't open your link.. 

R.E.Rourke
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project