From: nick Date: Sat Sep 01 05:48:37 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Dear Wayne, I use both, according to size of bit/drill etc. My comments about buying cheap electrobonded tools are based upon the apparent attrition rate of the more expensive bits on this particular job. Why wreck a $10 bit when a 30c bit will do under the same circumstances. I use Shell Ilocut oil for my bigger saws, a water soluble for my smaller ones and water on my drills etc as generally I have to due to the materials I work with. One of my students (day job) is doing research on a new bonding method for abrasives in metal that is rather interesting, simple as a plating bath but has the more precise profiles of a sintered product and greater depth of abrasive than the normal coated products so has nearly the tool life of a sintered continuous bonded product at a fraction of the cost. Nick ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project