    I've been presented the opportunity to buy a second-hand(used once)
    water torch and wondered if I could ask for some advice from the
    group?! 

    Mainly, I fabricate earrings and pendants out of sterling silver but
    I hope to expand this to include gold and PMC. I've been using a hand
    held butane torch to date. I'm not keen on having large canisters of
    gas at home but I do find it difficult to use the hand held with
    small soldering jobs - this is why I'm curious about the Water torch. 


    Is a water torch suitable for an amateur? Will I find the flame too
    small? I realise that I still need something else for annealing,
    would the combination of my hand held and a water torch be enough for
    most jewellers needs? 

    I've only just started out so have an awful lot to learn!!! I would
    greatly appreciate some advice from the group. 

    Here is a link to the water torch: http://tinyurl.com/3ckdr3 

    Anyone using this model out there.....how do you find it??? 

Kind regards
Corrina
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project