From: Al Balmer Date: Thu Aug 30 07:22:23 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Test a piece first. Liquid nitrogen will indeed harden flexible plastic, but the tubing may be easily shattered while cold, especially if you're trying to drill it. I worked for a research lab where the boss used vinyl tubing to demonstrate the effects of liquid nitrogen to visitors. A second in the flask, then rap it against the bench. It would shatter in a hundred pieces. Being something of a joker, he usually concluded his talk on the dangers of the stuff by dipping his hand in the Dewar flask and flinging a handful at them. (Safe enough - it forms an insulating layer of gas instantly.) Al Balmer Sun City, AZ ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project