    In my experience rhodium is one of the more difficult solutions to
    master. I'm by no means a chemist but I can tell you that rhodium is
    very acidic and is contaminated by the copper in sterling which will
    leach into the rhodium. Use a high karat gold handling wire or
    stainless steel, if using copper be very sure it is also nickel
    plated. When trouble shooting with customers I can tell you that
    cleaning is the most over looked, taken for granted step(s). A small
    particle of rouge will also quickly contaminate rhodium.
    Additionally, keep in mind that Elecrocleaner is a Base, so be sure
    to always use Acid Dip after the Electrocleaner because it will also
    negatively effect your rhodium solution. One last point and I'll quit
    babbling, each solution should have it's own dedicated distilled
    water rinse. "Always have two beakers and beaker covers for each
    solution" is what I tell my customers. 

Hope this helps,

Thackeray Taylor
Rio Grande Technical Support
800-545-6566
505-839-3000 ex 13903
technicalsupport AT tbg.riogrande.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project