From: Wayne Emery Date: Wed Aug 29 08:38:04 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Noel, There are many ways to achieve the speckled or mottled patinas. One way is to use sawdust (think coarse, medium or fine) which has been dampened with the appropriate solution (not soaked). The sawdust is placed along with the piece in a sealed container (Zip lock will work) and NOT MOVED for a few minutes or hours or overnight. Experimentation is in order, room temperature plays a part. Some creative thinking about the materials which come in contact with your metal piece can lead down lots of fun roads, not all explored thoroughly. Have fun! Wayne Emery ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project