Umesh,namaskar

    rhodium over silver -sure,but why? if you are strengthening it and
    already using sterling as your base metal it's a waste of rhodium
    solution in my opinion. Fine silver:unless you are making sushi
    sets, or sambar thali's in which case the rhodium or platinum would
    be fine as a protectant from high salt based sauces is equally
    unecessary..why not just plate with silver on silver to hide any
    solder seams,etc..? cheaper,same colour, and easily rationalized! 

    plating silver jewelry with gold underplate = another waste of
    solution.. Unless your BASE metal is nickle,one needs no plating over
    any of it unless it's purely asthetic,or you got a new digital plater
    and you want to play with it..again,a waste of solution,but if you
    have deep pockets plate away..but to what end???? What exactly are yo
    u trying to accomplish? 

R.E.Rourke
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project